Abstract
由於氧化鋯陶瓷在醫療應用中優異機械性質、優異的耐磨性與良好化學穩定性,這些特性使氧化鋯成為人體內硬組織的修復與植入物的適合材料而備受關注,目前已應用在人工髖關節的股骨頭和牙齒修復。然而氧化鋯材料對細胞和組織的親和力較差與生物活性較不良,因此,本研究目的是添加高活性矽酸鈣(10、20、30 wt%)於氧化鋯,再使用高溫爐燒結生坯,然後爐冷至室溫,來觀察相分析與微觀結構,評估材料的力學性能和降解特性(低溫降解與體外浸泡)。SEM、XRD、FTIR及EDS和親水性分析複合植入物表面的結構與組成。從研究結果顯示,隨著矽酸鈣的增加,強度有顯著的差異,氧化鋯雙軸強度從1300 MPa下降到330 MPa,三點彎曲強度則是590 - 136 MPa;隨著矽酸鈣的含量增加接觸角從57 °下降到36 °;從SEM圖像中可發現,矽酸鈣的增加使氧化鋯複合材料顆粒變大;XRD分析在30 wt%可明顯看到矽酸鈣的特性繞射峰;EDS也證明矽酸鈣成分之增加。除了機械與物理化學性質分析,還測試體外浸泡與低溫降解,結果顯示隨著時間增加強度稍微下降; 降解後表面顆粒大小些許變大。透過以上分析本研究矽酸鈣的添加有效地改善氧化鋯親水性以及降低其高強度。
Excellent wear resistance and good chemical stability due to excellent mechanical properties of zirconia ceramics in medical applications, These properties make zirconia a suitable material for repair and implants. It has been used in artificial hip joints and dental restoration of the femoral head. However, zirconia materials have poor affinity for cells and tissues and poor biological activity. Therefore, the present study was to add a highly active calcium silicate (10,20,30 wt%) zirconia, Sintering the green body using a high temperature furnace, Then the furnace is cooled to room temperature, To observe phase analysis and microstructure, Degradation of mechanical properties and characteristic evaluation of materials (low degradation in vitro degradation). SEM, XRD, FTIR and EDS analysis and hydrophilic implant surface structure of the complex and composition. From the research results, With the increase of calcium silicate, there are significant differences in strength, The zirconia biaxial strength ranges from 1300 MPa to 330 MPa, The three-point bending strength is 590 - 136 MPa; As the increase of the content of calcium silicate contact angle decreased from 57 ° to 36 °, From the SEM image, it can be found that Increase of calcium silicate zirconia composite oxide particles becomes large; In addition to mechanical properties and physical and chemical analysis, Also tested for in vitro soaking and low temperature degradation, The results show a slight decrease intensity increases with time. After degradation, the surface particle size becomes slightly larger. Through the above analysis, the addition of calcium silicate in this study effectively improves the hydrophilicity of zirconia and reduces its high strength, and has potential development in implants.
Subjects
氧化鋯
矽酸鈣
低溫降解
zirconia
calcium silicate
low temperature degradation
Type
thesis
File(s)
No Thumbnail Available
Name
107CSMU5592005-001.zip
Size
5.21 MB
Format
Unknown
Checksum
(MD5):d28e5a4c9023e98a1921b5bd104a7921