SUE-HONG WANG2026-10-162026-10-162019-06-01Pure ID: 15025413Pure UUID: 96f309b0-40c1-429e-9835-bdfd4f98f69510.1016/j.rinp.2019.102224https://www.scopus.com/pages/publications/85063744193https://scholars.csmu.edu.tw/handle/123456789/22450A cross-linked polymer was formed by the reaction between chitosan (Cs) and xanthan gum (XG) at a weight ratio of 1:1. XG-Cs/Ni nanowire (XG-Cs/-Ni) was prepared by adding nickel nanowires (Ni, -Ni) into XG-Cs to form a nano-magnetic polymerization colloid. The results of SEM and TEM analysis showed that the diameter of the nickel nanowires is approximately 80 nm and the length is approximately 11 μm, with a high density and aspect ratio. The (1 1 1), (2 0 0), and (2 2 0) crystal planes were analyzed by XRD. The magnetic nanowires were measured on a vibrating sample magnetometer at 300 K. A perpendicular magnetic field was applied to the substrate, where coercivity was 685 Oe and the squareness was 0.866. An applied parallel magnetic field of the substrate revealed a coercivity (118 Oe) and a squareness (0.068). XG-Cs/-Ni was mixed, and its coercivity was determined to the range from 914 to 957 Oe. The melting points (59.0–197.3/695.5 °C) of XG-Cs/-Ni were measured by differential scanning calorimetry. Thermogravimetric analysis of XG-Cs/-Ni revealed three weight loss points. Furthermore, XG-Cs polymers support cell adhesion and proliferation of 3 tested cell lines, XG-Cs polymers show significant cytocompatibility.enPreparation and physicochemical and cytocompatibility analyses of a magnetic polymer colloid of xanthan gum-chitosan/nickel nanowiresjournal article