曾惠馨Hui-Hsin Tseng林奕辰Yi-Chen Lin職業安全衛生學系2026-10-059999-12-312019https://handle.ncl.edu.tw/11296/5ycwm7https://scholars.csmu.edu.tw/handle/123456789/20482蛋白質常存在於生技產業或食品產業廢水而造成水處理薄膜積垢問題,降低薄膜分離性能。兩性離子因能有效提升薄膜吸附水分子能力,而成為薄膜提升抗蛋白質積垢能力的新興改質劑之一;唯受限於兩性離子與薄膜間的改質技術,使其抗蛋白質積垢能力仍有大幅改善的空間。故本研究開發一新型聚苯乙烯丙烯酸(acrylate-terminated polystyrene, SMA-HEA)連接劑,以有效的將兩性離子連接於聚偏氟二乙烯(polyvinylidene difluoride,PVDF)膜的表面,增強PVDF薄膜表面的親水性能形成水合層而提升其抗蛋白質積垢能力。SMA-HEA連接劑係由聚苯乙烯-馬來酸酐(polystyrene-maleic anhydride, SMA)嵌段共聚物和丙烯酸-2-羥乙酯(2-hydroxyethyl acrylate, HEA)聚合而成,故可以透過SMA嵌段之苯環與PVDF薄膜產生疏水性相互作用力,而提供錨定於PVDF薄膜的位點;此外,於HEA嵌段上具有裸露於結構外側之C=C雙鍵,可透過自由基聚合,共價鍵結磺基甜菜鹼甲基丙烯酸酯(sulfobetaine methacrylate, SBMA)兩性離子,而成為薄膜與兩性離子之間的橋樑。本研究分別先以表面吸附法及混合法嫁接兩性離子連接劑,後再以熱誘導式自由基聚合法連接兩性離子,並評估最佳吸附/聚合條件。改質後的薄膜以傅立葉紅外線轉換光譜儀(FTIR)、水接觸角分析儀、膜孔徑分析儀及掃描式電子顯微鏡進行分析,並進行靜態蛋白質吸附及動態蛋白質過濾試驗,以評估薄膜改質成效。研究結果顯示,改質後薄膜的接觸角由135°下降至27.7°,薄膜平均孔徑亦從106 nm減少至18.7 nm。靜態吸附及動態過濾試驗結果顯示,蛋白質吸附量從112.5減少至近似於0 μgcm-2;純水回復率由65 %提升至100 %,且蛋白質阻絕率達98 %,表明了改質後薄膜具有高親水性能有助於抗蛋白質積垢,而膜孔徑的收縮有助於阻絕率的提升。最後,以核磁共振(NMR)及FTIR分析推測兩性離子連接劑有助於高分枝狀兩性離子薄膜的形成。Protein foulants have existed in biotechnology and food industry wastewater, which lead to severe membrane fouling and decline membrane separation ability. Thus, a new hydrophilic material, zwitterions, can enhance membranes to adsorb water molecular and become an excellent anti-protein adsorption modifier. However, the methods of zwitterions modified process are unclear, that cause the anti-protein adsorption performance are limited. In this study, a novel strategy of connecting zwitterions to polyvinylidene difluoride (PVDF) membrane via a novel linker, acrylate-terminated polystyrene (SMA-HEA), is reported to enhance the PVDF membrane hydrophilicity and antifouling resistance. The SMA-HEA linker consisted of a polystyrene-maleic anhydride (SMA) block copolymer and 2-hydroxyethyl acrylate (HEA). The hydrophobic polystyrene moiety is adsorbed on membranes via hydrophobic-hydrophobic adsorption and anchored the grafted sulfobetaine methacrylate (SBMA) zwitterion. In contrast, the C=C bond of HEA provides a grafted site that connected with zwitterions by covalent bond. Above all, the connection performance of linker is demonstrated. First of all, to evaluate the best adsorption/polymerization condition. Connecting PVDF membrane and SMA-HEA linker via surface adsorption and blending process, then using the free radical polymerization process grafted zwitterion on the SMA-HEA linker. Moreover, the membrane characteristics such as hydrophilicity, pore size distribution, and antiprotein adsorption are analyzed. The results indicated that the modified membrane showed a decreasing water contact angle (WCA) from 135° to 27.7°, a decline pore size from 106 nm to 18.7 m, and a decreasing protein absorption from 112.5 to nearly 0μgcm-2. For filtration performance, the pure water flux recovery rate (FRR) enhance from 65% to 100%, and the protein rejection reach to 98%. These evidence display the excellent hydrophilic membrane can reduce protein adsorption and narrow pore size can enhance the separation of protein foulants. At the end, the SBMA polymerization mechanism of the SMA-HEA-linked PVDF membranes was determined by nuclear magnetic resonance (NMR) and Fourier transform infrared (FTIR) spectroscopies, and a branch-like zwitterionic structure of the PVDF-a-SMA-HEA-p-SBMA membrane was proposed. The PVDF membrane fouling resistances before and after modification were also analyzed.PVDF膜抗蛋白質吸附兩性離子高分枝狀連接劑廢水處理PVDF membraneanti-protein adsorptionzwitterionicbranch-like zwitterions linkerwastewater treatment.多節點SMA-HEA兩性離子連接劑開發及其於提升PVDF膜抗積垢性能之應用thesis