TSUI-HSIEN HUANGSHINN-JYH DING2026-10-162026-10-162007-11-25Pure ID: 15451839Pure UUID: 676e97b1-460d-4e52-9d13-c9590b607b1810.1016/j.surfcoat.2007.05.056https://www.scopus.com/pages/publications/35348867993https://scholars.csmu.edu.tw/handle/123456789/24663To improve the titanium-ceramic bonding is a challenged theme because the bonding plays an important role in long-term performance of dental prosthetic implants. This study focused on the pre-heat treatment effect on the surface characteristics of titanium and the bond strength of the porcelain-titanium system. Phase, morphology, and oxide layer thickness of the pre-heat-treated titanium were evaluated. In particular, the bond strength of porcelain fused to pre-treated titanium was measured by using three-point bending test. Statistical analyses were made using one-way analysis of variance (ANOVA). The results revealed that with an increase in treatment temperature, the intensity of diffraction peaks of rutile-type titania formed on pre-treated titanium surface increased. With regard to the thickness of the oxide layer, a monotonous change with increasing treatment temperature was observed. The bond strength of the porcelain-titanium system was 27.6 MPa for untreated titanium, which is above the minimum value of 25 MPa specified in ISO 9693 standard for the three-point bending test. When titanium subjected to pre-heat-treatment at 600-850 °C, the values became the range of 23.7-34.5 MPa, indicating significant differences (p < 0.05). The highest value resided in the optimal pre-treatment temperature of 750 °C at which specimens also presented greater amounts of remained porcelains on the titanium side among all tested groups after bending test. On the basis of the data, the pre-heat treatment in air for titanium substrates might be a simple and effective method for strengthening the titanium-ceramic bonding.6enEffect of preoxidation of titanium on the titanium-ceramic bondingjournal article